Challenges Customer Faced:
Delamination of different components in the multi-shot part and 2nd shot light colored material melting the 1st shot dark colored material dues to similar melt temperatures

KORE solutions:
We advised the change of materials to those with different melt temperatures to improve chemical bonding and miminize the discoloration of 2nd shot by the first due to melting.